Hydrothermal confinement and delignification assisted silicate stabilization enhance surface hardness and suppress set recovery in plantation grown Chinese fir

Kuai, Bingbin, Huang, Yuxuan, Zhang, Xuexia, Yang, Rilong, Guo, Fei, Yu, Yan
European Journal of Wood and Wood Products · Springer Nature · 2026-11-02 · DOI: 10.1007/s00107-026-02512-3

Аннотация

Surface densification can improve the surface performance of low density plantation wood, but moisture induced recovery of the compressed layer limits its dimensional stability. Here, localized surface hydration and asymmetric platen heating were combined with partial delignification and sodium silicate impregnation to produce and stabilize a surface densified layer in plantation grown Chinese fir while retaining a lower density core. Hydrothermal confinement generated an effective densification depth of 4.2–5.3 mm within the final 18 mm thickness. For the hydrothermal confinement series, an initial confinement temperature of 140 °C increased surface hardness from 708 N in untreated wood to 1784 N, with apparent dry-state recovery of 47.3% after the third wet-dry cycle. The maximum mean MOR of 85.8 MPa occurred at 120 °C. Partial delignification followed by sodium silicate impregnation was associated with greater surface hardness and lower apparent dry-state recovery. Among the tested combined treatment conditions, 6 h of delignification provided the preferred balance between mean surface hardness (2161 N) and apparent dry-state recovery (19.3%) after three wet-dry cycles. Extending delignification to 10 h further lowered apparent dry-state recovery to 9.9% but reduced hardness to 1674 N, indicating a trade off between lower apparent dry-state recovery and surface hardness. Whole specimen mass loss and impregnation associated dry mass gain increased with delignification time. X-ray photoelectron spectroscopy (XPS) detected silicon containing species in the post press surface region. The results demonstrate that moderate localized delignification combined with sodium silicate impregnation can promote surface consolidation and substantially reduce apparent dry-state recovery without densifying the entire wood cross section.

Читать у издателя →

Похожие статьи