Journal of the Indian Academy of Wood Science Науки о растениях
Using Fraké (Terminalia superba) wood waste to manufacture epoxy matrix composites for sustainable development
Аннотация
This study focuses on the development of a composite made from Fraké ( Terminalia superba ) wood waste in the form of particles and an epoxy matrix for use in industry. The composites are manufactured with three particle sizes ([t0.35[; [0.35–0.63 [; [0.63–1[) and three mass reinforcement percentages (50, 60 and 70%). Contact pressure moulding is used to produce the composite. Physical tests were carried out using a gravimetric and mechanical technique in accordance with ASTM D790—3. Due to the hydrophilic nature of Fraké particles, moisture content, water absorption and porosity increase, however, density decreases with increasing reinforcement content and particle size. The Page model best fits the experimental drying and absorption points for all formulations. The amount of energy required to remove water from composites (54–83 kJ.mol^−1) for wet and hot applications is highest at a reinforcement rate of 50%. Desorption diffusion coefficients increase with the addition of temperature during drying and are related to the porosity of the material. Mechanical properties such as Young's modulus (69–131 MPa) and mechanical strength (1–5 MPa) are highest at a reinforcement rate of 50% and a particle size of [t−0.35 [ mm and remains below the recommendations of standard EN 312 as a structural material. ANOVA statistical analysis shows a significant difference between size and reinforcement content. The increased performance at 50% reinforcement and a size of [t− 0.35[ mm suggests future applications in the automotive and construction sectors for low stress applications (computer supports, telephone booth doors, partitioning materials) and thermal insulation materials.