Fatigue and Fracture of Engineering Materials and Structures Машиностроение
Rolling Contact Fatigue Damage and Subsurface Microstructure Change of a Case‐Carburized CSS‐42L Steel
Аннотация
ABSTRACT To elucidate the rolling contact fatigue (RCF) failure mechanism of case‐carburized CSS‐42L gear steel, a plasto‐elastohydrodynamic lubrication (PEHL) model incorporating hardness gradients and surface roughness was integrated with twin‐roller RCF tests at 4.5–6.0 GPa. The maximum von Mises stress occurs at the subsurface. Because carburizing hardens the case and thus improves elastic load‐bearing capacity while suppressing plastic strain accumulation, the gradient model predicts a higher maximum von Mises stress but lower plastic and residual stresses than the homogeneous model. Higher contact pressure enlarges the plastic zone and asperity contact area ratio, shortening RCF life; life at 5.0 GPa is about 4.8 times that at 6.0 GPa, and carburizing extends life by at least 9.4 times at 4.5 GPa compared to original material. Subsurface spalling dominates the failure, and electron backscatter diffraction (EBSD) shows that carburizing increases dual‐carbide (M 7 C 3 and M 6 C) content within an ultrafine martensite matrix, enhancing RCF resistance.