Abstract Anode‐free sodium metal batteries (AFSBs) are regarded as a promising candidate for the next‐generation high‐specific‐energy storage systems due to their high energy density and simple preparation process. However, their practical application is limited by issues such as sodium dendrite growth, bulk transport‐desolvation mismatch, increased polarization, and rapid capacity fading. This perspective highlights the latest progress by Chen et al. ( Sci. Adv. , 2026), who proposed a spatially anion‐confined electrolyte (SAE) strategy. In this strategy, introducing positively charged nanoparticles into the electrolyte to anchor anions selectively generates local contact ion pairs that dominate the solvent, promoting rapid desolvation of sodium at the electrode interface and forming an anion‐derived solid electrolyte interphase (SEI). Simultaneously, solvent‐separated ion pairs around the nanoparticles maintain rapid ion transport in the bulk electrolyte, collectively enabling flat, high‐density sodium deposition at high current densities. Based on this strategy, the Na(Ni 1/3 Fe 1/3 Mn 1/3 )O 2 (NFM) || Al full cell provides an energy density of 415.6 Wh kg −1 at 1 C, with a capacity retention rate of 70.2% after 400 cycles. This work provides a new strategy for balancing bulk transport and interfacial kinetics and offers guidance for the research of other alkali metal batteries.

Читать у издателя →

Похожие статьи